Why not use 403 stainless?  Because 316 is a much better choice.

----- Original Message ----- From: "BRIAN ROSS" <rossbt verizon net>
To: "et" <Elec-trak cosmos phy tufts edu>
Sent: Saturday, June 10, 2006 3:52 PM
Subject: Re: (ET) panels


Why not use 403 stainless steel (muffler steel).
--- Neil Dennis <wombatt gmail com> wrote:

If I was making new panels, I'd use "terneplate" for
the sheet metal, got a pretty well acid proof lead coat already
there..

wombat